Check the dryfilm to etch dwell time. Also lighting and racking techniques and locations if the sat for any long length of times. (Sounds like dryfilm related) Groovy ______________________________ Reply Separator _________________________________ Subject: Plated Through Hole Rim Voids Author: [log in to unmask] at SMTPLINK-HADCO Date: 12/18/95 10:30 PM We have experienced a random problem with three or four parts relative to rim voids. In some cases it was part of the lot and in others it was the whole lot. They have been partial, full, top and or bottom. (no consistency) They are typically one to two mils down from the surface copper and one to three mils in height. They are not specific to any hole size. We use Dupont APG715 Dry Film, and develop on a Atotech/Chemcut horizontal system using Potassium Carbonate. I would appreciate any suggestions, as to the cause.