With regard to the question of flux compatibility to OSP finishes, it seems that a major concern / misunderstanding in the industry is that no clean pastes and fluxes will not solder well to OSP finished pads. We have tested and documented the compatibility of several water clean and no clean materials to both OSP and LPISM surface finishes. Testing criteria conformed to IPC-SM-840B, Ansi/J-STD-001, MIL-P-28809A and Martin Marietta Quality Specs. These documents are readily available through Enthone-OMI Inc. I hope the above is not considered too commercial. The intent is to provide the forum with information regarding OSP solderability with various flux type materials. Happy Holidays! Tom Eshelman, Enthone-OMI 1.800.548.9801 ext. 7257 [log in to unmask]