Terpenes may work better for you than Axarel. Petroferm makes terpenes for use in batch cleaners and benchtops. One warning is that the fumes from the terpene can be very offensive to some people after prolonged exposure. ______________________________ Reply Separator _________________________________ Subject: Cleaning of Roger's Duriod 6002/6010 Material Author: [log in to unmask] at cc_gate Date: 11/21/95 12:52 PM We are currently using Duriod 6002/6010 type PWB's on one of our products and are having problems cleaning the PWB's after soldering and assembly operations. Removal of fluxes and the cleaning fluid (Axarel) from this very hygroscopic material has been difficult inspite of using the Manufacturers recommended process. Any information or sources of potential information relating to resolving this situation would be appreciated. [log in to unmask]