Gloria: If the boards are solder levelled with no gold, you may want to ask your board supplier to re-solder level them, provided also that they are not teeny boards (less than 3" X 3"). The only risk you run from re-levelling after the board is cut out from the panel is a fracturing of the edges. Try taking a solderability sample per the IPC spec. Tom Coyle Field Services Engineer HADCO Corporation