That would depend largely on what solvent system and what urethane. We do not see issues with the urethane we use. Doug Pauls Principal Materials and Process Engineer Rockwell Collins On Mon, Nov 12, 2018 at 9:59 AM Ekaterina Stees <[log in to unmask]> wrote: > Happy Monday TechNetters! > > I was wondering if anyone has seen urethane conformal coating adversely > react with latex and/or nitrile gloves. > > Thank you, > Kate Stees >