Hi Ben - yes, there are differences in the mechanical properties and the solder joint microstructures for the "high temp" alloys. Most of those alloys have applications in component construction, specifically in component die attachment. One very common alloy used frequently in a number of applications is the 10Sn88Pb2Ag alloy. Dave Hillman Rockwell Collins [log in to unmask] On Thu, Sep 20, 2018 at 6:40 AM, Gumpert, Ben <[log in to unmask]> wrote: > TechNetters, > > J-STD-006 has a series of 'high temp' SnPb alloys (some with Ag) that are > close in SOL/LIQ temps. I'm familiar with Sn10Pb90 as a common high-temp > ball on ceramic BGAs, but I haven't seen the others used. Are there any > differences (e.g. mechanical properties) among these that would drive > selection, other than the SOL/LIQ? > Are some alloys more readily available than others? > > Ben >