IPC New Release: IPC-WP-024
IPC-WP-024 is a white paper which discusses the issues associated with reliability of smart textiles (e-textiles structures) following multiple washing cycles and emphasizes efforts that industry and research laboratories must undertake
to make e-textile structures more robust and able to be washed similarly to everyday textile products (e.g., underwear, clothing, home textiles and technical textiles).
The researchers provide initial reliability results of laboratory testing for e-textiles after multiple washing cycles in a commercially available washing machine and using common laundry detergents.
20 pages. Released August 2018.
Download:
Member Price: $25.00
Industry Price: $25.00
This white paper is available for sale only and is not available as a free member document.
Single-Device DRM-Protected Document
This document has single-device digital rights management (DRM) protection. Users of this document will only be able to open it on a single device. If you are purchasing this DRM-protected document for
another user, you will need to provide contact information for that user when placing your order.
For information about IPC standards with DRM protection, visit
www.ipc.org/drm.