Peter: The answer is "it depends" (insert eyeroll here) I worked at one place where we could use any cheap scanner through our conformal coating. Success depends on: The size of the smallest scannable barcode feature The thickness of the coating. (thicker is worse) Reflectivitiy of the coating and ambient light. If you're using a thin coat of Humiseal 1B73 and use a code 128 with 10 mil min feature size, you should be able to scan it with just about anything. I've worked on some designs where the 1B73 spec was 2mm thick. With thicker coatings and a dense 3 mil DataMatrix code, you'll have serious challenges getting anything reasonably priced to scan it. If it's a thick coating, your best bet is to mask it or move to RFID. Another option to explore, I haven't used them yet, but Microscan ( http://www.microscan.com) has some interesting high-res scanners. A quick way to see if it's your scanner or your barcode is to download a barcode scanner app on your phone. There are plenty of free ones out there. Best, Stephen Golemme Manufacturing Engineer 650-214-5647 x.company On Tue, May 8, 2018 at 2:48 PM, Elson, Ryan(BHGE) <[log in to unmask]> wrote: > We updated our conformal coating programs (selective spray) to avoid our > 2D barcodes, both label and laser engraved. I didn't investigate other > barcode scanners at the time as it seemed easier to modify our programs > than to buy a bunch of new scanners. For 2D matrix barcodes in general, > I've had good success with a Zebra DS4308 XD. But I don't know if it would > work well through coating. > > Thanks, > Ryan Elson > Manufacturing Engineer > Bently Nevada > Baker Hughes, a GE company > > Cell +1 775 790 5182 > > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter Wong > Sent: Tuesday, May 08, 2018 2:20 PM > To: [log in to unmask] > Subject: EXT: [TN] Barcode scanners through conformal coating > > We are printing 2D Aztec barcodes on Brady thermal transfer labels made > out of polyimide material and applying these onto our circuit assemblies. > > We then apply conformal coat (Humiseal 1B73 or 1A33) on the assemblies and > also the label. Our current barcode scanner, Zebra DS2208, cannot read the > labels after coating. > > What make and model of scanners are you using successfully for this > situation? > > Thanks > Peter > ________________________________ > The enclosed documents are proprietary items to Silicon Forest > Electronics' (SFE) customers. They shall not be reproduced nor disclosed > for any purpose except as specified in writing from an authorized agent of > SFE. These documents may contain data restricted for export by the > International Traffic in Arms Regulations (ITAR) section of the Arms Export > Control Act (or the Export Administration Act). Violators are subject to > severe criminal penalties. > This e-mail, and any file attached to it, is meant only for the intended > recipient of the transmission and may be a communication privileged by law. > If you have received it in error, please notify the sender immediately and > delete the original from your system. Any other use of this e-mail by you > is strictly forbidden. >