Victor, As much as I hate Librarying, I generally look for ~10% side, toe and ~20% heel . So for a 20 mil wide lead I would use 24 mils for minimum width and increase length by 6 mils (2 in front and 4 in back). If you want to dive deeper into the geometry of a solderjoint you can calculate some tighter numbers (lead height = pad expansion for side fillets to be 45 degree filled) The IPC calculator for land patterns will give you better numbers but for a quickie check I use the above as minimums Good luck, FNK Frank N Kimmey CID+ Electrical Engineer/PCB Design Verifone 1400 W Stanford Ranch Road Rocklin, CA 95765 T: 916-625-1818 M: 916-833-9877 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask] Sent: Friday, April 06, 2018 7:23 AM To: [log in to unmask] Subject: [EXT] [TN] FW: IPC Guideline for Gull Wing lead PWB pad to component lead ratio Fellow TechNetters: I don't have a part number nor spec, I only have the sample PCIe LF connector, 164 gull wing pins soldered onto a test board. I there a simple Rule Of Thumb for selecting a suitable PWB pad side which will yield an acceptable toe, heel and side negative solder wetting angle? Victor, From: Hernandez, Victor G Sent: Tuesday, April 3, 2018 10:00 AM To: TechNet E-Mail Forum <[log in to unmask]> Cc: Hernandez, Victor G <[log in to unmask]> Subject: IPC Guideline for Gull Wing lead PWB pad to component lead ratio Fellow TechNetters: Can someone point me in the right direction for PWB SMT pad dimensions for gull wing devices? Heel LF solder fillet formation concern. Victor, ********************************************************* This electronic message and any attachments are intended only for the use of the addressee. The information in this electronic message is confidential and proprietary, and may include privileged information. If you are not the intended recipient, please delete this electronic message and any attachments and notify the sender of the error. Please be aware that any unauthorized use, dissemination, distribution or copying of this message or any attachments is strictly prohibited.