A few solutions we have been offering are to * Pre-coat critical components in a hydrophobic coating before actual assembly * Pre-apply a hydrophobic coating around the connectors before application. * Apply the hydrophobic coating to masking boots This gives the components or masking some ability to "reject" the conformal coating being applied due to the change in surface tension and certainly can reduce incidence of capillary. Contact me offline for more details. Best Regards Dr Lee Hitchens Please be aware that I am personally based in Thailand and travel frequently due to business. If I am unavailable you can also contact my offices directly in the UK, USA and India for support. Mob: +66 95 418 5931 Skype: leehitchens UK: +44 1226 249 019 India: +91 900 038 3674 USA: +1 206 257 9787 www.conformalcoating.co.uk SCH Technologies is a Division of SCH Services Limited On 08/02/2018 10:01, Richard Kraszewski wrote: > Yup Real common for unsealed connectors. > > You either have to find a better masking solution (often not possible) and/ or use multiple layers of a highly atomized (dry ) spray that is not very mobile when it hits the PCBA. > > Some unsealed ZIF connector styles where the requirement is coat the leads but contacts are all KOZ are really a problem for me due to capillary action of the coating if still wet when it hits the PCBA. > > > > Rich Kraszewski > Senior Staff Process Engineer > Plexus Engineering Solutions > * * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * * > > This e-mail and any attachments are confidential from Plexus Corp. and may contain information which is privileged, confidential, and/or protected by non-disclosure agreements. They are intended solely for the use of the named addressee(s). . Any unauthorized use or disclosure may be unlawful. If you are not a named addressee, you must not use, disclose, retain or reproduce all or any part of the information contained in this e-mail or any attachments If you have received this transmission in error, please destroy it and notify us immediately by return e-mail or by calling + 1 888 208 9005. > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson > Sent: Wednesday, February 07, 2018 4:17 PM > To: [log in to unmask] > Subject: Re: [TN] IPC-CC-830 (Conformal Coat) > > sorry for the long delay (and thank you for the responses) but as I was reviewing these posts I had another question: > > Have you ever heard of problems with conformal coating material wicking up the connector leads and causing intermittent connections? > > thanks again, > Jack > > > On Wed, 6 Dec 2017 14:09:46 -0500, lduso - Diamond-MT.com <[log in to unmask]> wrote: > > (..snip...) >> It's up to me to decide how close to J1 to get with the coating. I once >> coated the leads of all the fine-pitch connectors and the customer said >> that was too close. The next customer will reject the work if I don't >> coat the leads.