Totally know just where you are coming from, Ken. I did the same, and now my kids after me. Wouldn't trade that experience for anything, and I receive thanks from my kids for the same every day. Wish my Dad were here to see them, but I have faith he does. dean -----Original Message----- From: Ken Barton [mailto:[log in to unmask]] Sent: Tuesday, September 05, 2017 3:52 PM To: TechNet E-Mail Forum; Stadem, Richard D. Subject: RE: [TN] [EXTERNAL] Re: [TN] Multilayer PCB of Different Substrat Thickness RF Design "... he eeeaaaarrned it!" LOL I think so, 17 yrs old, Dad (layout guy at Litton G&C) referenced me to the fab shop where over almost two years I worked in all depts. Can still smell the ammonia, toluols & hysol blue powder. Part of my job was to treat these aluminum cores, drill & fill then laminate. Ken Barton CID Technical Designer, Avionics HW Blue Origin, LLC 21218 76th Avenue S. Kent, WA 98032 (253) 437-5625 x625 [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D. Sent: Tuesday, September 05, 2017 1:40 PM To: [log in to unmask] Subject: Re: [TN] [EXTERNAL] Re: [TN] Multilayer PCB of Different Substrat Thickness RF Design I agree with Joyce, Ken became an excellent design engineer by broadening his horizons the old-fashioned way, he eeeaaaarrned it! dean -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Yuan-chia Joyce Koo Sent: Tuesday, September 05, 2017 3:23 PM To: [log in to unmask] Subject: Re: [TN] [EXTERNAL] Re: [TN] Multilayer PCB of Different Substrat Thickness RF Design aha, someone paid the dues... consider you are endangered species... hard to come by... pat on your back... On Sep 5, 2017, at 2:23 PM, Ken Barton wrote: > I worked at two different fab houses, well before I went into layout > design. Not as a "plan", just how it went, & I now consider the > experience, particularly for design work invaluable. > > Ken Barton CID > Technical Designer, > Avionics HW > > Blue Origin, LLC > 21218 76th Avenue S. > Kent, WA 98032 (253) 437-5625 x625 > [log in to unmask] > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Yuan-chia Joyce > Koo > Sent: Tuesday, September 05, 2017 10:45 AM > To: [log in to unmask] > Subject: [EXTERNAL] Re: [TN] Multilayer PCB of Different Substrat > Thickness RF Design > > i always believe to send designer to fab house for 6 month (even 3 > month) will do a world of good... > On Sep 5, 2017, at 1:32 PM, Dwight Mattix wrote: > >> Fun times that. Unbalanced in material thickness + single sided >> sequential lam to get the last core into the stack. Hope you have an >> experienced fabricator who is willing to plan some extra time into >> the process for long press cool down and a flatbake after. >> Don't rush that. >> >> Also, hope you're prefilling the blind via in the 62 mil core with a >> non-conductive epoxy (e.g. San-Ei PHP). Doubt 4450 is going to have >> volume of free resin needed for that. >> >> -----Original Message----- >> From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory >> Sent: Tuesday, September 5, 2017 10:21 AM >> To: [log in to unmask] >> Subject: Re: [TN] Multilayer PCB of Different Substrat Thickness RF >> Design >> >> Hi Ricardo, >> >> I finally have your picture posted, Richard was right, had some >> pressing things on the production floor to take care of after the >> long weekend. >> Here's your stack-up drawing: >> >> http://stevezeva.homestead.com/Ricardo_Stackup.jpg >> >> Steve >> >> On Tue, Sep 5, 2017 at 7:50 AM, Stadem, Richard D. >> <[log in to unmask] >>> wrote: >> >>> Hi, Ricardo >>> >>> I do not have the capability to post your picture, but I am sure >>> Steve can, and I see you have copied him. >>> >>> Being that many people are taking vacations here this week as part >>> of Labor Day weekend, not sure when Steve will be in. You may need >>> to wait until later today. >>> >>> In looking at the stack-up, I do not have a lot of expertise in this >>> area, but I do know that having differing layer thickness can maybe >>> cause some issues with different coefficients of thermal expansion >>> during reflow and other heat excursions. This can put stresses on >>> the vias passing all the way through the board. But I am not an >>> expert in those issues. One suggestion; you would be wise to also >>> pose the question to the Designers Forum. I am sure they can give >>> you plenty of advice on that. >>> >>> Richard >>> >>> >>> >>> *From:* Ricardo Moncaglieri [mailto:[log in to unmask]] >>> *Sent:* Tuesday, September 05, 2017 8:34 AM >>> *To:* Stadem, Richard D.; Steve Gregory >>> *Subject:* Re: Multilayer PCB of Different Substrat Thickness RF >>> Design >>> >>> >>> >>> Steve, Richard, >>> >>> Would you pls upload the herebelow quoted image inord to be more >>> clear on my quetion to the forum? >>> >>> Indeed hope to receive your comments / advise. >>> >>> Keep awaiting. >>> >>> Thank you very much, brgds,Ricardo >>> >>> >>> >>> ------------------------------------------------------------ >>> ------------------------------------------------------------ >>> -------------------------------------------------------------------- >>> - >>> >>> Estimated colleagues, >>> >>> Nice to get in contact again with all of you after a bit long time. >>> >>> We are deploying a RF design and by first time we intend to use a >>> multilayer pcb with different substrat thickness as shows the >>> stack-up herebelow detailed. >>> >>> Questions here are: >>> >>> As per your experience, is it recomendable such a kind of substrat >>> design? >>> >>> Some pcb provider reported it is very difficult to achieve. Can you >>> recommend or share your background about pcb provider who can assure >>> high reliability on this pcb provision? >>> >>> Keep awaiting for your unvaluable feedback. >>> >>> brgds, Ricardo >>> >>> Ricardo Moncaglieri >>> >>> QA Electronic Service Manager >>> >>> INVAP SE >>> >>> www.invap.com.ar >>> >>> >> >> >> -- >> Steve Gregory >> Kimco Design and Manufacturing >> Process Engineer >> (208) 322-0500 Ext. -3133 >> >> -- >> >> >> This email and any attachments are only for use by the intended >> recipient(s) and may contain legally privileged, confidential, >> proprietary or otherwise private information. Any unauthorized use, >> reproduction, dissemination, distribution or other disclosure of the >> contents of this e-mail or its attachments is strictly prohibited. If >> you have received this email in error, please notify the sender >> immediately and delete the original.