Hi Steve, The only reason I asked about stencil thickness was because the last time I dealt with a BGA connector was with a MOLEX HD Mezzanine connector. Their recommendation was to use a 6-mil thick stencil. I had 0402's and some fine pitch QFP's on the board that just couldn't take a 6-mil thick stencil, so I had my stencil vendor etch down everything EXCEPT the connector footprint from 6 to 4 mils, so I was able to print the 0402's and fine pitch with no issues and print the 6-mils recommended by Molex. Wished I had a MY500 Jet printer, but didn't have the bucks 😀 Never had any problems with them http://www.molex.com/pdm_docs/as/AS-45802-001-001.pdf Steve On Tue, Aug 29, 2017 at 6:38 AM, Steven Kelly <[log in to unmask]> wrote: > Hi All, > > The connector supplier is the one who told us this was dried flux > residue- the pictures may not be the best but these joints are duller than > the surrounding joints. > > The stencil /profile is per the connector manufacturer’s recommendation. > > We have built approx.. 20 parts to date. 14 have no issues . The other 6 > have 1-3 head pads each with head in pillow issues – no pattern to the > failure. We have traced two failures to “dull joints”. > > > > Regards Steve Kelly > > > > > > *From:* Steve Gregory [mailto:[log in to unmask]] > *Sent:* August-28-17 6:12 PM > *To:* [log in to unmask] > *Cc:* Ed Popielarski <[log in to unmask]>; Steven Kelly < > [log in to unmask]> > *Subject:* Re: [TN] Dried flux > > > > Hi Steve, > > Sorry it's taken me so long to get you pictures posted, but I had to sort > out some issues with the software for my web page. Windows 10 and all it's > updates made things a little difficult for a while, but I've gotten things > straightened out now. Here are your photos: > > http://stevezeva.homestead.com/partial_ball_thumb.jpg > > http://stevezeva.homestead.com/dull_solder.jpg > > http://stevezeva.homestead.com/Head_in_pillow_1.jpg > > http://stevezeva.homestead.com/Head_in_pillow_2.jpg > > To be honest, I'll have to take your word for it but I couldn't see any > flux residues in your photo. They must be there, I just can't see them. May > I ask how thick the stencil is that you're printing the paste with? Just > curious is all. Also, who makes the connector? > > Steve > > > > > > On Mon, Aug 28, 2017 at 7:50 AM, Steven Kelly <[log in to unmask]> wrote: > > Thanks Steve for posting these for me. > The first picture called partial ball is a picture of one of the balls on > the connector as received. > Second picture is what the supplier has called dried flux on the > connector as received > Third picture shows what we call head in pillow > Fourth picture - different view of third picture > > Thanks for everyone's help on this . Regards Steve Kelly > > > -----Original Message----- > From: Ed Popielarski [mailto:[log in to unmask]] > Sent: August-25-17 2:26 PM > To: TechNet E-Mail Forum <[log in to unmask]>; Steven Kelly < > [log in to unmask]> > Cc: Steve Gregory <[log in to unmask]> > Subject: RE: [TN] Dried flux > > Steve Gregory (cc'ed herein) has graciously offered his time and dataspace > to post Technet pix on his site. > > Forward your pics to Steve, I'm certain he will oblige! > > Regards, > > Ed Popielarski > Engineering Manager > > > 970 NE 21st Ct. > Oak Harbor, Wa. 98277 > > Ph: 360-675-1322 > Fx: 206-624-0695 > Cl: 360-544-2289 > > > > “It's one kind of victory to slay a beast, move a mountain, and > cross a chasm, but it's another kind altogether to realize that the beast, > the mountain, and the chasm were of your own design.” > https://goo.gl/maps/mMjg43rXeFB2 > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Kelly > Sent: Friday, August 25, 2017 11:13 AM > To: [log in to unmask] > Subject: Re: [TN] Dried flux > > Hi all, > Want to post some pictures - can someone please give me direction. Thanks. > Steve Kelly > > -----Original Message----- > From: Bev Christian [mailto:[log in to unmask]] > Sent: August-25-17 11:00 AM > To: 'TechNet E-Mail Forum' <[log in to unmask]>; Steven Kelly < > [log in to unmask]> > Subject: RE: [TN] Dried flux > > Steve, > From what people are saying, it is more and more likely that it IS the > flux residue. You say: "On average we are getting 1-3 failures per 200 > joints." That pretty well eliminates gross part warpage. > > Minor point of interest: > With regards to part warpage (or boards), they can test fine for planarity > both before and after reflow. That doesn't mean they weren't warped DURING > reflow. > Bev > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Kelly > Sent: Friday, August 25, 2017 10:26 AM > To: [log in to unmask] > Subject: Re: [TN] Dried flux > > Hi Dave, > The parts come vacuum sealed and after opening we have a fairly short > period of time to assemble. Manufacturer also said the “dull ball” on the > connector is common for lead-free solder ( agree) and is not considered > related to the failure. Its’ mainly because tin constituent appears on the > surface. ( I understand that) Then they say the “residue” which we > identified on the ball is considered to be flux and is not related to the > head in pillow. > But only a few of the 200 or so balls exhibit this issue and I am not > saying we do not have other issues but we have traced some of the head in > pillow to a couple of the so-called flux residue balls . On average we are > getting 1-3 failures per 200 joints. > We have measured the flatness of the rigid stiffener – looks OK to us – > co-planarity is .002- .004 after convection reflow. > Reviewing what Bev said yesterday- pasting – we looked at it 3 times but > doing it again. > I also have pictures of what we call an incomplete ball which I would like > to post but I need a refresher course on how to do this. > > Thanks for everyone’s help. > Steve Kelly > > From: David Hillman [mailto:[log in to unmask]] > Sent: August-25-17 10:06 AM > To: TechNet E-Mail Forum <[log in to unmask]>; Steven Kelly < > [log in to unmask]> > Subject: Re: [TN] Dried flux > > Hi Steve - We use a number of "bga style" connectors where there is a > solder charge/preform on the connector which is designed to combine with > the solder paste deposit creating sufficient solder volume and good solder > joint integrity. I am not familiar with the having these types of > connectors with "dried flux" - flux has a shelf life so the manufacturer's > comment doesn't make much sense. From a practical point, the flux in the > solder paste deposit is doing the bulk of the oxide scrubbing action so > dried flux contribution is most likely a moot point. But - the fact that > the manufacturer did not acknowledge the possible shelf life issue is > dis-concerning. > > Dave Hillman > Rockwell Collins > [log in to unmask]<mailto:[log in to unmask] > > > > On Thu, Aug 24, 2017 at 1:11 PM, Steven Kelly <[log in to unmask]<mailto: > [log in to unmask]>> wrote: > Hi All, > I have a new hi-density BGA connector I am trying to assemble. When the > supplier makes the connector they "solder balls onto the pin" (lead free). > We see dried flux on the balls and when we solder the connector we are > getting a few joints with head in pillow. The connector manufacturer says > the dried flux is not an issue - is this true? Thanks. Steve Kelly > > > > > -- > > Steve Gregory > > Kimco Design and Manufacturing > > Process Engineer > > (208) 322-0500 Ext. -3133 <(208)%20322-0500> > > > > > > This email and any attachments are only for use by the intended > recipient(s) and may contain legally privileged, confidential, proprietary > or otherwise private information. Any unauthorized use, reproduction, > dissemination, distribution or other disclosure of the contents of this > e-mail or its attachments is strictly prohibited. If you have received this > email in error, please notify the sender immediately and delete the > original. > -- Steve Gregory Kimco Design and Manufacturing Process Engineer (208) 322-0500 Ext. -3133 -- This email and any attachments are only for use by the intended recipient(s) and may contain legally privileged, confidential, proprietary or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly prohibited. If you have received this email in error, please notify the sender immediately and delete the original.