Hi Frank, IEC 62137-1-1 Pull strength test (GW leads) IEC 62137-1-2 Shear strength test Those standards give you the test method (like pull and shear speed) and also how to assess the results. But hey do not give any value of strengths as a reference. Gabriele -----Messaggio originale----- Da: TechNet [mailto:[log in to unmask]] Per conto di Frank Kimmey Inviato: lunedì 28 agosto 2017 23:39 A: [log in to unmask] Oggetto: [TN] Solder Joint Shearing Force I need to know if there is standard shear force measurement for SMD solder joints. We need to run some experiments and need a starting place. Any help is appreciated in advance. Thanks, FNK Frank N Kimmey CID+ Electrical Engineer / PCB Design VeriFone Inc 1400 W Stanford Ranch Road, Suite 200 Rocklin, CA 95765 USA W: 1-916-625-1818 M: 1-916-833-9877 [log in to unmask] ********************************************************* This electronic message and any attachments are intended only for the use of the addressee. The information in this electronic message is confidential and proprietary, and may include privileged information. If you are not the intended recipient, please delete this electronic message and any attachments and notify the sender of the error. Please be aware that any unauthorized use, dissemination, distribution or copying of this message or any attachments is strictly prohibited. --- Questa e-mail è stata controllata per individuare virus con Avast antivirus. https://www.avast.com/antivirus