I am considering requesting capital for an additional or replacement XrF system, but would like to go in armed with a short list of particular models and costs and be confident of their performance records and capabilities. The least important factor is cost, so don't hold back from sending me a confidential email on your choice. The machine should be able to accurately determine the percentage of gold, silver, tin, nickel, lead, copper, etc., down to the .001% level in order to confirm that the plating on incoming component leads meets the component print or requirements. It should also be able to accurately determine the metallurgic make-up of any given metal sample. Is that asking a lot? I don't know. I prefer a hand-held, but if what I am looking for is only available in a base machine package, then that will have to work. No information you folks provide will be shared. Feel free to send me an email at either [log in to unmask]<mailto:[log in to unmask]> or [log in to unmask]<mailto:[log in to unmask]>. I sincerely appreciate any information you can share with me. Thanks R. Dean Stadem