how large is your pcb? panel or singulated? if it is already singulated and not large size, you can use manual hand print with squeege. prototype? 3-5 units? or you produce for qual - 20 to 30 unit? On Jun 8, 2017, at 6:42 PM, Bob Cochran wrote: > Hi, > > We want to bring in house a high quality, low cost manual stencil > printer for prototyping / reflowing several of the same PCB in a > batch run. > > There are many, many models out there to choose from, but the > specifications seem to be limited. > > If you can recommend one, please do so. And if there are ones to > stay away from, then please share this, too. > > Thank you, > > Bob Cochran > > > -- > Robert E. Cochran > Mind Chasers Inc. > https://mindchasers.com > 297 Route 72 W, Suite 35-315 > Manahawkin, NJ 08050