There is an application where a flex circuit will mate with a Gold plated ZIF connector. The finish on the flex will ideally be platinum. Does anyone foresee any issues at the gold/platinum interface? Both metals will have a nickel barrier underneath. Thank you, Mike Lehmicke Project Engineer DSS Division Molex, LLC-Printed Circuit Solutions 22 Empire Drive St. Paul, MN 55103 651-846-7728 [log in to unmask]<mailto:[log in to unmask]> [cid:[log in to unmask]][cid:[log in to unmask]]<http://www.molex.com/> ________________________________ CONFIDENTIALITY NOTICE: This message (including any attachments) may contain Molex confidential information, protected by law. If this message is confidential, forwarding it to individuals, other than those with a need to know, without the permission of the sender, is prohibited. This message is also intended for a specific individual. If you are not the intended recipient, you should delete this message and are hereby notified that any disclosure, copying, or distribution of this message or taking of any action based upon it, is strictly prohibited. English | Chinese | Japanese www.molex.com/confidentiality.html