I guess you’re looking for some way of getting the grunge to be soluble. Makes sense, since at least its constituents were at one time. Maybe try some Bismuth? I don’t know which low melting point metals make the best solvent. From: Nutting, Phil [mailto:[log in to unmask]] Sent: Tuesday, March 07, 2017 10:37 AM To: Wayne Thayer; TechNet E-Mail Forum Subject: RE: grunge at bottom of tinning solder pot Yup, in every solder pot that does not get proper maintenance. From: Wayne Thayer [mailto:[log in to unmask]] Sent: Tuesday, March 07, 2017 1:36 PM To: TechNet E-Mail Forum; Nutting, Phil Subject: RE: grunge at bottom of tinning solder pot Superior adhesion and hardness, with a relatively low temperature process! Can you replicate this stuff? -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Nutting, Phil Sent: Tuesday, March 07, 2017 10:32 AM To: [log in to unmask]<mailto:[log in to unmask]> Subject: Re: [TN] grunge at bottom of tinning solder pot If it were so simple. The pots were typically run very hot and for long periods with only the dross on the top of the solder skimmed off. No one ever scraped the side walls of the crucible so now there is rock hard, non-melting crud that defies removal. -----Original Message----- From: Stadem, Richard D. [mailto:[log in to unmask]] Sent: Tuesday, March 07, 2017 1:25 PM To: TechNet E-Mail Forum; Nutting, Phil Subject: RE: grunge at bottom of tinning solder pot I assume you can turn on the pot and melt the solder, then scoop both the molten solder and the crud out, scrape it clean, fill it with fresh solder and send it out for analysis, if it passes continue production, update the maintenance schedule, and go from there. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Nutting, Phil Sent: Tuesday, March 07, 2017 12:13 PM To: [log in to unmask]<mailto:[log in to unmask]> Subject: [TN] grunge at bottom of tinning solder pot I have two wire tinning solder pots that have not received the proper day-to-day maintenance and now there is solid crud filling all but about ¼ of the crucible. I have tried chiseling it out and drilling it out. All I end up with is dull tools, even carbide drills. Other than buying new solder pots or replacing the crucibles are there any suggestions for removing this super hard stuff? Phil Nutting | HVP Development Engineer | Excelitas Technologies Corp Lab: +1 978.224.4332 | Office: +1 978.224.4152 35 Congress St, Salem, MA 01970 USA [log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]:[log in to unmask]>> www.excelitas.com<http://www.excelitas.com><http://www.excelitas.com/> [Excelitas R_emailsig] Please consider the environment before printing this e-mail. ________________________________ This email message and any attachments are confidential and proprietary to Excelitas Technologies Corp. If you are not the intended recipient of this message, please inform the sender by replying to this email or sending a message to the sender and destroy the message and any attachments. Thank you.