Absolutely, provided a proper calibration for it is established. I’m pretty sure how to go about it is described in IPC 4556 (either in the body of the document or in one of its Appendices). José (Joey) Ríos, Sr QA Engineer Mission Assurance Kavli Institute for Astrophysics & Space Research Massachusetts Institute of Technology [log in to unmask] <mailto:[log in to unmask]> (617)324-6272 > On Feb 7, 2017, at 9:14 AM, [log in to unmask] wrote: > > Fellow TekNetters: > > Can Palladium, Pd, be identified in an alloy mixture such as Ni/Pd with a Fischer scope XRF Instrument? I have detected Pd as a layer by itself in the past. > > Victor,