IPC New Release: IPC-9241
Guidelines for Microsection Preparation
This standard is intended as a guideline in the proper preparation of a metallographic sample (microsection) of a printed board. The finished microsection is used for evaluating the quality
of the laminate system and plated structures (e.g. PTHs and vias). Microsection sample preparation is regarded by many as a highly developed skill. The guidelines in this standard discuss the many variables and problems associated with the process from sample
removal to micro-etch. The guidelines do not promote any one vendor’s process, but discuss the variables common to microsectioning.
44 pages. Released December 2016.
Preview the
table of contents .pdf file.
Hard copy:
Member Price: $75.00
Industry Price: $148.00
IPC members may request a free single user download of a document with digital rights management of each new standard by visiting
www.ipc.org/free-member-docs within 90 days. The file is enabled to print one copy of the standard. Please
note that you will receive the file from an e-mail from IHS.com. The file must be opened within 10 business days and will LOCK to the computer of the person who OPENS the file.