As a former pwb fab guy, we used to treat a lot as each individual ‘work order’ on the floor. We would not group all individual fab work orders of the same p/n and treat them as a single lot because there is typically mix of processing dates (lamination dates, drill dates, plating dates, and so on). I think the generally accepted definition is something along the lines of: "lot is a group of parts processed together and presented for inspection at the same time". 6012 for example, defines sampling plans in Table 4-3, the table specifies also whether the sampling is lot based (once per lot), panel based or individual pwb based. José (Joey) Ríos, Sr QA Engineer Mission Assurance Kavli Institute for Astrophysics & Space Research Massachusetts Institute of Technology [log in to unmask] <mailto:[log in to unmask]> (617)324-6272 > On Dec 14, 2016, at 3:39 AM, Bush, Brien <[log in to unmask]> wrote: > > You can refer to sampling standards at ANSI/ASG Z1.4 > > > Experience the benefits of Precision Engagement > > Brien Bush > Manufacturing Applications Specialist > Phone: 603.249.9190 | Fax: 603.249.9192 > [log in to unmask] www.cirtronics.com > > > ISO 9001 & 13485 Certified > Follow us on LinkedIn|Friend us on Facebook > > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Lehmicke, Michael > Sent: Tuesday, December 13, 2016 11:03 PM > To: [log in to unmask] > Subject: [TN] Definition of the word lot in IPC-6013 - Bayesian Filter detected spam > > When IPC-6013 talks about acceptance testing, it references a sampling plan per # of parts in a "lot". > > I am curious what the definition of a "lot" is. Can anyone help? > > Mike > > Mike Lehmicke > Project Engineer > DSS Division > Molex, LLC-Printed Circuit Solutions > 22 Empire Drive > St. Paul, MN 55103 > 651-846-7728 > [log in to unmask]<mailto:[log in to unmask]> > > [cid:[log in to unmask]][cid:[log in to unmask]]<http://www.molex.com/> > > > ________________________________ > > > > CONFIDENTIALITY NOTICE: This message (including any attachments) may contain Molex confidential information, protected by law. If this message is confidential, forwarding it to individuals, other than those with a need to know, without the permission of the sender, is prohibited. > > This message is also intended for a specific individual. If you are not the intended recipient, you should delete this message and are hereby notified that any disclosure, copying, or distribution of this message or taking of any action based upon it, is strictly prohibited. > > English | Chinese | Japanese > www.molex.com/confidentiality.html > WARNING: Export Control This message, including any attachments, may contain technical data within the definition of the International Traffic in Arms Regulations (ITAR), and subject to the Export Control Laws of the U.S. Government. Transfer of such information by any means to a foreign person, whether in the United States or abroad, without proper export authorization or other approval from the U.S. Department of State is prohibited.