Well, Cu shouldn't diffuse through a layer of E-Ni to begin with!: Any difference in diffusion rate and or temperature/time above liquidus will only affect the thickness of intermetallics, which isn't that much of importance for typical values. Regards, Vladimir Sent from my BlackBerry 10 smartphone on the Rogers network. Original Message From: Stadem, Richard D. Sent: Thursday, November 10, 2016 15:28 To: TechNet E-Mail Forum; Vladimir Subject: RE: [TN] Immersion Tin - problems Not so fast. While the dwell time and temperature in the selective solder process plays a huge role in determining the amount of copper leaching, so does the finish. If the plating, such as ENIG, uses a nickel barrier, the amount of copper pad leaching away is greatly reduced. The nickel barrier protects it somewhat. In that case the IMF is formed with the nickel, not the copper. Immersion Tin typically does not have any barrier; it is plated directly to the copper similar to OSP or immersion silver. As soon as the immersion tin is absorbed into the molten solder, the leaching of the basis copper begins. Not so much with ENIG or ENEPIG, both of which have the nickel barrier. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Vladimir Sent: Thursday, November 10, 2016 12:17 PM To: [log in to unmask] Subject: Re: [TN] Immersion Tin - problems Hi Juliano, The board finish most probably has nothing to do with the problem. It must be your process. Regards, Vladimir SENTEC Sent from my BlackBerry 10 smartphone on the Rogers network. Original Message From: Datacom - Juliano Ribeiro Sent: Thursday, November 10, 2016 13:13 To: [log in to unmask] Reply To: TechNet E-Mail Forum Subject: [TN] Immersion Tin - problems Hello to all, We recently are changing to Lead Free process to specific products and we need to change the finishes boards from (HAL Tin Lead) to Immersion Tin. But during the Selective Soldering process the component pad is damaged. Are there limitation about Immersion Tin about Max. Temperature, Max. Reflow/Wave process, Max Soldering Contact Time, etc.??? In this case the HAL Lead Free is better? Thank you Juliano Ribeiro