Hi folks - lots of good comments, just one more to add: copper diffuses faster than nickel so some folks increase their reflow temperatures 5-10C and/or slow down the belt speed 3-6 inches per minute. It isn't necessary to do this but it does have some good metallurgical basis. Werner Englemaier used to advocate doing this when a board finish involved nickel (Werner and I discussed this at length, very fun conversations). I set my reflow profile based on the board thermal characteristics and the solder paste material but being aware of the plating metallurgy impacts (such as the gold embrittlement Wayne detailed) is always a good idea. Dave Hillman Rockwell Collins [log in to unmask] On Thu, Nov 10, 2016 at 1:33 PM, Jose A Rios <[log in to unmask]> wrote: > The reflow profile is typically not a function of the final finish of the > pwb. If it is thats news to me. > > José (Joey) Ríos, Sr QA Engineer > Mission Assurance > Kavli Institute for Astrophysics & Space Research > Massachusetts Institute of Technology > [log in to unmask] <mailto:[log in to unmask]> > (617)324-6272 > > > > > On Nov 10, 2016, at 2:17 PM, Wayne Thayer - EXT <[log in to unmask]> > wrote: > > > > Those two finishes are fairly similar from a wettability perspective, > assuming the ENIG is done properly and that no contamination or significant > oxidation occurs. > > > > If you are putting down some high-Au parts, such as leadless ceramic > packages, then the reduction in solder volume will make joint > embrittlement/stalled flow (due to AuSn being formed) more likely, so you > may want to adjust stencil apertures if you have those parts. > > > > But profile should probably be good. Might be able to reduce time above > liquidus slightly to reflect the fact that with ENIG there is no oxide to > strip. > > > > Wayne > > > > -----Original Message----- > > From: TechNet [mailto:[log in to unmask]] On Behalf Of Blair Hogg > > Sent: Thursday, November 10, 2016 11:01 AM > > To: [log in to unmask] > > Subject: [TN] Reflow Profile using HASL or ENIG > > > > Hi Technetters, > > > > Would a reflow profile need to change based upon the finish of the > board? If we switch from HASL to ENIG would we need to change any > parameters? (I know, probably too broad of a question) > > > > Thanks! > > > > Blair >