That is really good to know. To all of you who responded, thank you so much! I really don't know what we would do without the excellent people in Technet! -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of lduso - Diamond-MT.com Sent: Wednesday, October 05, 2016 10:22 AM To: [log in to unmask] Subject: Re: [TN] Silicone Conformal Coating supplier Another factor is that the fluorescence is not well dispersed so it does not resemble a very smooth color like 1B31. It will be mottled under the light but it is easy to see under white light. Lloyd Duso Plant Manager Diamond-MT (814) 535-3505 www.Diamond-mt.com On Wed, Oct 5, 2016 at 11:15 AM, Douglas Pauls < [log in to unmask]> wrote: > Dean, > We use Dow Corning 1-2577 as our approved silicone and it has always > worked well for us. It is about 20-30% toluene, so it is a VOC, but > if memory serves, there are low VOC versions of 1-2577 out there. > While it does have a relatively quick tack time, you may want to bake > it a while to drive the cure reaction and improve adhesion. > > > Doug Pauls > Principal Materials and Process Engineer Rockwell Collins > > On Wed, Oct 5, 2016 at 10:08 AM, Wayne Thayer - EXT < > [log in to unmask] > > wrote: > > > Isn't that stuff about half toluene? > > > > Really--I love 1-2577 too, but won't it cause all of the "VOCs" > > alarms in the county to go off at once? > > > > Wayne Thayer > > > > -----Original Message----- > > From: TechNet [mailto:[log in to unmask]] On Behalf Of lduso - > Diamond-MT.com > > Sent: Wednesday, October 05, 2016 7:54 AM > > To: [log in to unmask] > > Subject: Re: [TN] Silicone Conformal Coating supplier > > > > 90% of our customers (DOD & commercial) call out Dow 1-2577. A good > > all around SR that is extremely easy to apply, t/u, rework and has a > > very > quick > > "dry" time of a mere 20 minutes @ room temp. Others are MG Chemicals > > and Humiseal. > > > > Lloyd Duso > > Plant Manager > > Diamond-MT > > (814) 535-3505 > > www.Diamond-mt.com > > > > On Wed, Oct 5, 2016 at 10:48 AM, Stadem, Richard D. < > > [log in to unmask]> wrote: > > > > > I have a client who needs to qualify a silicone coating, either an > > > oven cure or UV cure coating. I am looking for a good supplier or > > distributor. > > > If any of you coating experts would care to share your favorites > > > with me, I would greatly appreciate it, as I am not an expert on > > > sources of coatings (best pricing, service, stocking, etc.) Feel > > > free to contact me directly by answering this email. > > > Thanks for any info you feel comfortable sharing. > > > dean > > > > > >