I have a question regarding using the high temp solder after removing standard solder Sn63/Pb37. After wicking away the standard solder, we need to re-solder the wiring and components using the high temp solder (Sn95/Ag5). We are concerned that the integrity of the solder joint and the temperature rating may be negatively affected. Is this a legitimate concern? Any suggestions? Regards, Mary Grace Keenan, Quality Assurance Manager Taber Industries 455 Bryant St. North Tonawanda, N.Y. 14120 [log in to unmask] Phone (716) 694-4000 Ext.134 Fax (716) 694-1450 *********************** DISCLAIMER *********************** This email message contains information from Taber Industries for the sole use of the intended recipient(s) and may contain confidential and privileged information. Any unauthorized review, use, disclosure is prohibited. If you are not the intended recipient, please contact the sender by reply email and destroy all copies of the original message. Any data attached may contain information subject to the ITAR or EAR. This information may not be exported, released, or disclosed to foreign nationals without first complying with the export license requirements of the ITAR and EAR. While precautions are taken against computer viruses, it is your responsibility to scan for their presence and we accept no liability or responsibility therefore. Thank you. *********************** DISCLAIMER ***********************