I also think that the distributor of the solderability tester (Obrien) sells small bottles also. Rich Kraszewski (920) 969-6075 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of David Hillman Sent: Wednesday, May 11, 2016 7:33 AM To: [log in to unmask] Subject: Re: [TN] Alpha ROSIN (ROL1) Test Flux Hi Victor - if you are conducting solderability test per either the IPC- JSTD -002 or -003, the fluxes specified for testing are listed in one of the Appendices by product name/supplier. The specifications also list the flux chemistry constituents so that you can mix it yourself. One word of caution -there are dozens of ROL1 fluxes on the market but they do not meet the requirements of the JSTD specifications. Dave Hillman Rockwell Collins [log in to unmask] On Wed, May 11, 2016 at 7:26 AM, Victor Hernandez < [log in to unmask]> wrote: > Fellow TechNetters: > > Does anyone out there have a part number for the above solder type. > Need to conduct bare board solder float test, 1x. 3x and 6x. Ten second > intervals. > > Victor, > > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or > [log in to unmask] > ______________________________________________________________________ > ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________