One of the process variables that people always forget is time. "WE haven't changed anything, but our yield is way down " Then you find on investigation that there is a major undocumented change in that. Example from low volume line: Assemblies being stacked for batching. If production rate or batch size changes then the waiting time from first to last in the stack can also change considerably. Typically batch paste printed boards waiting to go to P&P or reflowed boards waiting for cleaner. It can have significant effect and produce nice intermittent fault rate. -- Regards Mike -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Yuan-chia Joyce Koo Sent: Thursday, May 26, 2016 4:37 PM To: [log in to unmask] Subject: Re: [TN] How much change is change? good old days: major change, any material change (including chip encapsulation, SMT adhesive if it is high speed cct or high temp), form fit function, MFG location change (medium - if set of tooling are equivalent and better, but just location change - electrical voltage of the tooling are different for example), any change of design rules - for example: on chip redundancy, vs. system redundancy using comparitor, critical components change - micro-processor for example, laser is another, etc. (optical always consider critical, or you risk in multiple way, wavelength, drifting, scattering, reflection, etc. Minor change, new tooling with same platform, but more throughput, new location, but same tooling (do a x-y plot, one location vs the other, it should come out with some correlation, in terms of yield, quality, etc.). down grade environmental requirement (do not use at design extreme), material from different MFG facility, but same vendor (you still need qual a bit - electrolytic cap from some neck of the woods use city water... even under same label... I was being picky to get one of my components from a specific site by paying a bit more... just don't want deal with un-certainty. components bin change but still met the requirement (spec tolerance). etc. (not much, the list much shorter than Major... the design don't want to take risk in legal sense... if design call the shot ). my 2 cents. (oh, my dear good old days... you finish and sign off on the dotted line, say good bye and matching to next project without scare for something come back to bit you... until scheduled review - usually 5 years for upgrade possible platform... I guess currently that kind of schedule are hard to come by). jk On May 26, 2016, at 10:59 AM, Douglas Pauls wrote: > Good morning all, > > One of the IPC groups that I am leading is presently wrestling with > the > issue of minor vs. major change. Generally along the lines that if > you > have a baselined or qualified manufacturing process, how much can that > process change before it needs to be re-baselined or re-qualified? > Sometimes this is referred to as Level 1 vs. Level 2 change. > > So far, every quality documentation system that I have looked at, like > AS9100, ISO9000, etc., gets really fuzzy and uses vague terms when you > approach this issue. Most of these documentation systems have change > better defined for products, but get extremely fuzzy and extremely > vague > about manufacturing processes. > > This forum has a lot of very smart, very experienced people. How > would you > differentiate a minor change, which would not impact form fit or > function, > from a major change, which "could/would" impact form fit or function? > > And I want all you lurkers to come out of the woodwork on this one. > > Doug Pauls > Principal Materials and Process Engineer > Rockwell Collins > > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud > service. > For more information please contact helpdesk at x2960 or > [log in to unmask] > ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________