What is temp cycle condition again? You have 50 to 125C but did you mean -50C to +125C? Also are you doing temp cycle or air/air temp shock (ie. what is ramp rate in chamber or better yet as measured on the product during temp cycle). Jim Maguire Intel Corporation ATD Q&R Stress Lab Operations Hawthorne Farms; Oregon Engineer Phone: 503-696-3309 Cell: 253-651-9373 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Ricardo Moncaglieri Sent: Monday, April 18, 2016 2:58 PM To: [log in to unmask] Subject: Re: [TN] Solder Cracking After Thermal Cicling Steve, Responding your question. Soldered connection is not put under vibration during temp cicling. This terminal belongs to a connector which is screwed on a case and its terminal passes through this metalic case and lyies on the pcb ENEPIG pad. So that there are following CTEs playing and intercating each other all together: PCB CTE Solder CTE Case CTE where is screwed the conector Terminal CTE brgds,Ricardo >>> Steve Gregory <[log in to unmask]> 18/04/2016 18:47 >>> Hi Ricardo, I finally have your pictures up, they are here: http://stevezeva.homestead.com/A15_Photos_of_pre__post_100_temp_cycling_CSC-10_SN12.pdf Boy, that looks like a big CTE mis-match. A question; are the boards going through ESS? Vibration along with the temp cycling? Steve On Mon, Apr 18, 2016 at 2:35 PM, Ricardo Moncaglieri < [log in to unmask]> wrote: > Steve, > Attached arethe pictures. > Thank you a lot. > Await for your comments. > brgds,Ricardo > > >>> Steve Gregory <[log in to unmask]> 18/04/2016 15:22 >>> > Hi Ricardo, > > The Technet server strips the attachments, send your photo directly to me > and I'll get it posted... > > Steve > > On Mon, Apr 18, 2016 at 11:43 AM, Ricardo Moncaglieri < > [log in to unmask]> wrote: > > > Dear colleagues; > > > > Steve Gregory, could you please upload the enclosed picture? > > > > Solder become perturbated / cracked after thermal cicling: > > > > This picture corresponds to a plane (not circular) conector terminal > > solded to a pcb pad ENEPIG finished. > > The connector terminal has been gold removed by twice pretin. > > Solder used is Sn63Pb37. > > Thermal cicling: 50°C to 125°C > > > > As picture showed there are stretch marks toward left direction and > > showed solder crack. > > > > Our provider reported temperature didnt pass over 125°C and solder used > > 63/37. > > > > Question: > > > > How could these kind of gooves or stretch marks have been produced > > taking into account they are just toward one direction (left) and of > > considerable length? > > Just mecanic stress? > > Temperature overpassing on any cicle? > > Need of use of different alloy, ie.: In, Bi etc? > > Provider reported the process is being useed from them since long ago > > (same solder alloy, temperature, pcb, terminal conector, thermal > > cicling) but this is the first time they faced with such a cracking. > > > > Do you have any comment in order to anlyse/solve this trouble. > > > > Appreciate your feedback we are in middle of a providing acceptance > > tests space quality level (IPC class 3). > > > > brgds,Ricardo > > > > > > > > ______________________________________________________________________ > > This email has been scanned by the Symantec Email Security.cloud service. > > For more information please contact helpdesk at x2960 or > [log in to unmask] > > ______________________________________________________________________ > > > > -- > > > This email and any attachments are only for use by the intended > recipient(s) and may contain legally privileged, confidential, proprietary > or otherwise private information. Any unauthorized use, reproduction, > dissemination, distribution or other disclosure of the contents of this > e-mail or its attachments is strictly prohibited. If you have received > this > email in error, please notify the sender immediately and delete the > original. > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ -- This email and any attachments are only for use by the intended recipient(s) and may contain legally privileged, confidential, proprietary or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly prohibited. If you have received this email in error, please notify the sender immediately and delete the original. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________