Environment does matter. If you are using in harsh or automotive environment, test the different options in temperature cycle testing. You will likely find the CA glues will fail. Some use an RTV. You should also consider tape dots. We found they exceeded the temp cycling requirements and do not have any curing to worry about. Look up wire dots from circuitmedic for example. We have used these for many years with no issues. Roger Mack P.Eng. Manufacturing Specialist Parker Hannifin Canada Electronic Controls Division 1305 Clarence Avenue Winnipeg, MB R3T 1T4 Canada direct 204 453 3339 x7373 [log in to unmask] www.parker.com/ecd From: "Stadem, Richard D." <[log in to unmask]> To: <[log in to unmask]> Date: 2016-04-13 08:30 AM Subject: Re: [TN] adhesive recommendation Sent by: TechNet <[log in to unmask]> It depends on the product type. Can you give us a little more info as to what the product is and its typical use environment? Also, is the board conformal coated? -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of pietro Sent: Wednesday, April 13, 2016 7:49 AM To: [log in to unmask] Subject: [TN] adhesive recommendation Hi. I'm new to the forum and hope my request make sense. When using jumper wires on PCB, besides other directives IPC recommend to put adhesive spot at least every 25.4mm. My basic question: is there any recommendation about what kind of glue/adhesive to use ? Any suggestion will help. Thanks Pietro ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ -- Pietro Vergine President CID Trainer Leading Edge Via Delle Attivitá 18 24041 Brembate (Bergamo) - Italy mobile (+39) 335-5783220 email: [log in to unmask] internet: www.leading-edge.it Skype: pietver27 Rispetta l'ambiente: se non ti è necessario, non stampare questa mail. To respect the environment, if not necessary do not print this email ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________