Steven, Vias that are filled and capped (IPC-4761 Type VII) are processed before any other through plated holes are drilled in the panel so the answer to your questions is yes. All you need to do is clearly specify your requirements on your fabrication documents. Regards, John Parsons -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Kelly Sent: March-31-16 11:30 AM To: [log in to unmask] Subject: Re: [TN] Selective Via fill By selective via fill I mean like a conductive or non-conductive fill that you would use in a via-in-pad application for a BGA as an example. Regards Steve -----Original Message----- From: Stadem, Richard D. [mailto:[log in to unmask]] Sent: March-31-16 2:12 PM To: TechNet E-Mail Forum <[log in to unmask]>; Steven Kelly <[log in to unmask]> Subject: RE: Selective Via fill You have several options that I know of: 1. Dispense a water-soluble maskant such as Techspray on the vias you do not want to fill with solder, then wave solder all of the other vias that you do want filled. You can also apply kapton tape dots. They come in pretty much any size you wish. 2. Skip the soluble masking or tape dots and just perform selective soldering. If there are vias close by that you do not want filled, mask only those. 3. Simply ask the PWB fabricator to plate shut the vias that you want filled. 4. Apply solder paste on those holes you want filled as part of the solder paste stencil printing process. The holes you want to be filled will require an aperture in the stencil. You can designate which ones you want to print paste onto and your stencil provider can add those apertures only to the stencil, along with the rest of the SMT apertures. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Kelly Sent: Thursday, March 31, 2016 1:03 PM To: [log in to unmask] Subject: [TN] Selective Via fill Hi All, Is there a selective via fill process available in the industry- e.g. - fill one via and then not fill another one .020 away on a circuit. Thanks. Steve Kelly ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ -- ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________