Also, If you saw what came out of a MY600 jet printer you would never want to use a stencil again. Stencils are very fast though, I would not try serious production runs on a MY600. Though, if you did, your solder paste would be perfect, or at least very close. Bob K. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Lawrence Dzaugis Sent: Thursday, March 24, 2016 2:32 AM To: [log in to unmask] Subject: Re: [TN] TN] Auger Driven Dispensers Assembling 3d circuit, one off circuits or unusually fabricated proto types. Guy Ramsey <[log in to unmask]> wrote: >You can add extra paste where needed when a step won't work. >Rework where stencils are difficult or impossible. > >On 3/23/2016 3:20 PM, Ahne Oosterhof wrote: >> Just curious, why would you use such a dispenser rather than a stencil? >> >> Ahne. >> >> -----Original Message----- >> From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Wettermann >> Sent: Wednesday, March 23, 2016 6:55 AM >> To: [log in to unmask] >> Subject: [TN] Auger Driven Dispensers >> >> Gents/Ladies: >> >> We are looking at putting a non-pneumatic drive dispenser on a robot. Due to some pretty fine dots, the need for speed and for consistency and the need for some lines to be dispensed, we are looking at an auger-driven system (5-6 mil dots). >> >> Does anyone have favorite vendors of the dispensing pumps and controllers that can be added on to a pieces of automation equipment? >> >> Regards >> >> >> _____________________________________________________________________ >> _ This email has been scanned by the Symantec Email Security.cloud >> service. >> For more information please contact helpdesk at x2960 or >> [log in to unmask] >> _____________________________________________________________________ >> _ >> -- >> Bob Wettermann >> BEST Inc >> [log in to unmask] >> Cell: 847-767-5745 >> >> _____________________________________________________________________ >> _ This email has been scanned by the Symantec Email Security.cloud >> service. >> For more information please contact helpdesk at x2960 or >> [log in to unmask] >> _____________________________________________________________________ >> _ > > >______________________________________________________________________ >This email has been scanned by the Symantec Email Security.cloud service. >For more information please contact helpdesk at x2960 or >[log in to unmask] >______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________