Doug, My former employer did not use ROSE for production monitoring. I know at least one board supplier provided SEC readings with every lot of bare boards. Most component manufacturers are good (clean components) , but some are still sketchy. Bev -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls Sent: December 4, 2015 11:57 AM To: [log in to unmask] Subject: [TN] ROSE on No-Clean Assemblies Good morning all, As you wrestle with Dave's element question, I have a question or questions for you. For those of you who are manufacturing product using no-clean technology and no cleaning, Do you do ROSE testing on the no-clean units and if so, do you consider the ROSE tested assembly still viable or is it scrapped? If you want to reply off-channel, that is fine. Thanks. Doug Pauls Principal Materials and Process Engineer Rockwell Collins ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________