Mike, Thanks for sending this link - that report was very interesting. Note that the detailed discussion of solder cracks along with interesting photos is also on page 66. Thanks, Howard Watson -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Buetow Sent: Tuesday, December 01, 2015 7:28 AM To: [log in to unmask] Subject: [TN] Airbus crash pinned (in part) on solder joint failures Here's the report: http://kemhubri.dephub.go.id/knkt/ntsc_home/ntsc.htm Discussion of the electrical short and cracked solder joint begins on page 104. Best, Mike Mike Buetow PCD&F/Circuits Assembly w/m: 617-327-4702 @mikebuetow The 2015 CIRCUITS ASSEMBLY *Directory of EMS Companies:* circuitsassembly.com/dems ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________