Hi Steve, I thought about how this might happen, and why sometimes bottom & sometimes top. If the board house has more than one copy of the mask artwork for each side, one of those sets might have the image looking like a donut instead of a pancake (hey, I don't work in a board house, so I'm using the best tools I can muster at this hour of the morning). Multiple photo tools could be used simultaneously in a case of very high volume so multiple imagers could be utilized for parallel processing. Just looking for a logical explanation. Ed Popielarski Engineering Manager 970 NE 21st Ct. Oak Harbor, Wa. 98277 Ph: 360-675-1322 Fx: 206-624-0695 Cl: 949-581-6601 “It's one kind of victory to slay a beast, move a mountain, and cross a chasm, but it's another kind altogether to realize that the beast, the mountain, and the chasm were of your own design.” https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: Wednesday, November 11, 2015 8:09 AM To: [log in to unmask] Subject: Re: [TN] Unusual solder mask defect... Hi James, This is a mixed technology board, so there is the SMT on the topside along with the through hole pattern. I don't know how the mask was applied. Steve On Wed, Nov 11, 2015 at 4:22 AM, James Head <[log in to unmask]> wrote: > Is this a common solder-mask pattern? I.e. is it a through-hole only > board that would have the same soldermask apertures on both sides of the board? > Was it an air-spray or curtain-coat application? > > Regards, > James > > James Head BEng CID+ MIIE MIET > Senior PCB CAD Engineer > Crowcon Detection Instruments Limited > 172 Brook Drive > Milton Park > OX14 4SD > Telephone: +44 (1235) 557700 ext. 7885 > E-mail: [log in to unmask] > > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or > [log in to unmask] > ______________________________________________________________________ > -- This email and any attachments are only for use by the intended recipient(s) and may contain legally privileged, confidential, proprietary or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly prohibited. If you have received this email in error, please notify the sender immediately and delete the original. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________