Phil, If all the strands were loose and not all soldered together I would say go ahead and crimp. But with all the wires soldered into a solid mass I think the crimping would be like trying to crimp to a large solid wire. I recall that is not an accepted practice. I think you have no option but to solder the Litz to the terminal but that will focus bending, and breakage, at the wire to solder transition. If the remain Litz is secured and there is little vibration probably ok. Now all that is my guessing to fill in the blanks I never knew or forgot. :-( Bob K -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Nutting, Phil Sent: Thursday, October 22, 2015 5:15 PM To: [log in to unmask] Subject: Re: [TN] to solder or not to solder Litz wire in crimp lug Bob, Yes, the stripping is accomplished by the tinning process as it "burns off" the Nylon thread serve and the enamel coating on each starnd. Chemical stripping brings in a whole bunch of issues we chose not to play with. Depending on the Litz wire and the frequency range of system operation the individual strands of wire could be as small as 40 to 48 gauge and lots of them. -----Original Message----- From: Robert Kondner [mailto:[log in to unmask]] Sent: Thursday, October 22, 2015 5:09 PM To: 'TechNet E-Mail Forum'; Nutting, Phil Subject: RE: [TN] to solder or not to solder Litz wire in crimp lug Hi, I would think you need to strip the Litz pror to crimping. The stripping is accomplished, I assume, in the tinning process. If you are tinning and stripping in one fell swoop in a solder pot then the Litz would come out as a rigid piece, not the best candidate for crimping into a terminal. So I probably missed something but how are you stripping the Litz? Chemically? How many fine strands are we talking? Bob K. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Nutting, Phil Sent: Thursday, October 22, 2015 4:30 PM To: [log in to unmask] Subject: [TN] to solder or not to solder Litz wire in crimp lug Esteemed colleagues, For our high voltage transformers, many are wound with Litz wire (see links below for more info). To make an electrical connection we tin the wire ends in a solder pot. From there the tinned wire may be inserted and soldered into a circuit board or a ring lug is crimped onto the tinned end. So here is the "discussion" within our group. I have fought (and won) to eliminate crimping and tinning of ring lug terminated regular stranded or solid wire. The theory being that if the crimp lug has been properly sized to the wire and the tool used is properly calibrated for the lug/wire being crimped that the crimp forms a gas tight seal and further treatment such as soldering it is unnecessary or even detrimental. I have supporting documentation from Amp for this statement. Ok, now enter tinned Litz wire. Does the properly sized lug/wire combination require soldering after crimping? Some here say it must be soldered the argument being the solder is softer than the copper and therefor there will be cold flow. Also if it heats up the solder could melt, but if that happens there are bigger problems than just the crimp/solder joint, IMHO. I believe crimping and tinning of Litz is not necessary, simply crimping is sufficient. Opinions? Reference links; https://en.wikipedia.org/wiki/Litz_wire https://www.newenglandwire.com/en/products/litz-wire-and-formed-cables/types -and-constructions Phil Nutting | HVP Development Engineer | Excelitas Technologies Corp Lab: +1 978.224.4332 | Office: +1 978.224.4152 35 Congress St, Salem, MA 01970 USA [log in to unmask]<mailto:[log in to unmask]> www.excelitas.com<http://www.excelitas.com/> [Excelitas R_emailsig] Please consider the environment before printing this e-mail. ________________________________ This email message and any attachments are confidential and proprietary to Excelitas Technologies Corp. If you are not the intended recipient of this message, please inform the sender by replying to this email or sending a message to the sender and destroy the message and any attachments. Thank you. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________