For sure you don't want bright and shiny nickel as you have. A good rule of thumb: Things that stay bright and shiny are hard to solder. Exception: Gold -- Regards Mike -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian Sent: Friday, October 30, 2015 12:10 AM To: [log in to unmask] Subject: Re: [TN] No-wetting on Mini USB (Nickel plating) Deng, I suggest if you have the time, get the supplier to provide you connectors with a tin or solder plating already on the connection pins. About a decade ago almost lost my job over these suckers. Told my boss that the USB connectors were bare nickel and he brushed it off and we had terrible field problems as a result. Bev Blackberry Opinions expressed are my own and may not represent those of the company I work for. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Deng RongJun Sent: October 29, 2015 3:33 AM To: [log in to unmask] Subject: [TN] No-wetting on Mini USB (Nickel plating) Hi Technetters I have got a problem with a SMT type mini USB connector. The four pins contacted shield are no-wetting after reflow soldering. But can be solder well by iron. The pins only plated by Nickel, is it possible the oxidation film creating on pin surface and then affect soldering? Picture: https://goo.gl/photos/qap1CBEWzUEJEc5i6 Thanks in advance. RongJun Deng ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________