Steve, There are a number of components that don't go well with conformal coating. Either the coating interferes with function, as Adrian indicates, or the components are not robust enough to withstand the solvents used. Adrian, you might consider a UV curable peelable mask, on the order of a Dymax EMAX 906B or Dymax 9-20515. We have decent success with those and they are much faster than latex masks. I tested both for residues and both are good. The 906B is thicker, the 9-20515 is thinner. Doug Pauls Principal Materials and Process Engineer Rockwell Collins On Thu, Sep 3, 2015 at 11:35 AM, Steve Gregory <[log in to unmask]> wrote: > Hi again, > > One question that I have to ask out of curiousity, why would you be masking > SMT components anyway, don't you want to coat them? > > Steve > > On Thu, Sep 3, 2015 at 10:30 AM, lduso - Diamond-MT.com < > [log in to unmask]> wrote: > > > Tape is used most of the time and we use blue 3m masking tape (low > > adhesion) on fragile components. If you are using a fine material like > 1B31 > > or other acrylics, then we may seal with latex if it is a connector that > > may "wick" easily. That's why I asked what coating you were using. > > > > Lloyd Duso > > Diamond-MT > > Plant Manager > > (814) 535-3505 > > www.Diamond-mt.com > > > > On Thu, Sep 3, 2015 at 11:23 AM, Adrian Dimulescu < > [log in to unmask] > > > > > wrote: > > > > > We're using Humiseal TS300 (Pink Bubble-Gum type), the lifting occurs > > when > > > we try to pick the mask from around and on top of the components. We > > tried > > > masking with tape and lining the tape with the Humiseal TS300, though > > this > > > works, it's time consuming. > > > > > > What material and technique do you use? > > > > > > Thanks > > > > > > -----Original Message----- > > > From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls > > > Sent: Thursday, September 03, 2015 11:01 AM > > > To: [log in to unmask] > > > Subject: Re: [TN] Selective Conformal Coat Systems > > > > > > I agree with Lloyd, if you are damaging components during demask, you > are > > > using the wrong materials and the wrong techniques. > > > > > > Trot them out here where we can see em and we'll help ya out. > > > > > > > > > Doug Pauls > > > Principal Materials and Process Engineer Rockwell Collins > > > > > > On Thu, Sep 3, 2015 at 9:55 AM, lduso - Diamond-MT.com < > > > [log in to unmask] > > > > wrote: > > > > > > > That sounds more like the problem, masking technique. We mask > hundreds > > > > a day and rarely damage anything. It's all in using the right > > > > technique and as Steve said, the right material. > > > > > > > > What coating are you using? > > > > > > > > Lloyd Duso > > > > Diamond-MT > > > > Plant Manager > > > > (814) 535-3505 > > > > www.Diamond-mt.com<http://www.Diamond-mt.com> > > > > > > > > On Thu, Sep 3, 2015 at 10:43 AM, Adrian Dimulescu > > > > <[log in to unmask] > > > > > > > > > wrote: > > > > > > > > > That’s what we’re doing now, the issue is removing the mask as it > > > > > will occasionally lift a pad or component. We’re looking to do > away > > > > > with masking. > > > > > > > > > > > > > > > > > > > > Thanks > > > > > > > > > > > > > > > > > > > > ------------------------------ > > > > > *Adrian Dimulescu | Advanced Engineer | MtronPTI (NYSE MKT: LGL)* > > > > > 2525 Shader Rd, Orlando, FL 32804 > > > > > Office: 407.298.2000 > > > > > > > > > > > > > > > > > > > > *From:* lduso - Diamond-MT.com [mailto:[log in to unmask]] > > > > > *Sent:* Thursday, September 03, 2015 10:41 AM > > > > > *To:* TechNet E-Mail Forum; Adrian Dimulescu > > > > > *Subject:* Re: [TN] Selective Conformal Coat Systems > > > > > > > > > > > > > > > > > > > > That low a volume, mask and spray by hand. > > > > > > > > > > > > > > > Lloyd Duso > > > > > > > > > > Diamond-MT > > > > > Plant Manager > > > > > (814) 535-3505 > > > > > > > > > > www.Diamond-mt.com<http://www.Diamond-mt.com> > > > > > > > > > > > > > > > > > > > > On Thu, Sep 3, 2015 at 10:39 AM, Adrian Dimulescu < > > > > [log in to unmask]> > > > > > wrote: > > > > > > > > > > Hello All, > > > > > > > > > > We're looking into purchasing a small (bench-top type) automated > > > > selective > > > > > conformal coat system. This will be used for 100 or so boards a > > > > > week, therefore speed is not an issue. It is important that the > > > > > system is selective as we only want to coat specific areas on the > > > > > board. I wanted > > > > to > > > > > get a feel for what other are using and/or recommend. > > > > > > > > > > Many Thanks > > > > > > > > > > > > > > > > > > > > CONFIDENTIALITY NOTICE: > > > > > This email together with any attachments is confidential; intended > > > > > for > > > > only the > > > > > recipient(s) named above and may contain information that is > > > > > privileged > > > > or > > > > > exempt from disclosure under applicable law. If you have received > > > > > this > > > > email in > > > > > error, or are not the named recipient(s), you are hereby notified > > > > > that > > > > any use, > > > > > dissemination, distribution or copying of this email or any > > > > > attachments > > > > is > > > > > strictly prohibited. Please immediately notify the sender and > delete > > > > this email > > > > > and any attachments from your computer. You should not retain, copy > > > > > or > > > > use this > > > > > email or any attachments for any purpose, or disclose all or any > > > > > part of > > > > the > > > > > contents to any person. The LGL Group, Inc. and its subsidiaries > > > > reserve the > > > > > right to monitor all email communications through its networks. > > > > > > > > > > > > > > > > > > > ______________________________________________________________________ > > > > This email has been scanned by the Symantec Email Security.cloud > > service. > > > > For more information please contact helpdesk at x2960 or > > > > [log in to unmask] > > > > > ______________________________________________________________________ > > > > > > > > > > ______________________________________________________________________ > > > This email has been scanned by the Symantec Email Security.cloud > service. > > > For more information please contact helpdesk at x2960 or > > [log in to unmask] > > > ______________________________________________________________________ > > > > > > > > > ________________________________ > > > Adrian Dimulescu | Advanced Engineer | MtronPTI (NYSE MKT: LGL) > > > 2525 Shader Rd, Orlando, FL 32804 > > > Office: 407.298.2000 > > > > > > > > > > > > > > > > > > > > > CONFIDENTIALITY NOTICE: > > > This email together with any attachments is confidential; intended for > > > only the > > > recipient(s) named above and may contain information that is privileged > > or > > > exempt from disclosure under applicable law. If you have received this > > > email in > > > error, or are not the named recipient(s), you are hereby notified that > > any > > > use, > > > dissemination, distribution or copying of this email or any attachments > > is > > > strictly prohibited. Please immediately notify the sender and delete > this > > > email > > > and any attachments from your computer. You should not retain, copy or > > use > > > this > > > email or any attachments for any purpose, or disclose all or any part > of > > > the > > > contents to any person. The LGL Group, Inc. and its subsidiaries > reserve > > > the > > > right to monitor all email communications through its networks. > > > > > > ______________________________________________________________________ > > > This email has been scanned by the Symantec Email Security.cloud > service. > > > For more information please contact helpdesk at x2960 or > > [log in to unmask] > > > ______________________________________________________________________ > > > > > > > ______________________________________________________________________ > > This email has been scanned by the Symantec Email Security.cloud service. > > For more information please contact helpdesk at x2960 or > [log in to unmask] > > ______________________________________________________________________ > > > > -- > > > This email and any attachments are only for use by the intended > recipient(s) and may contain legally privileged, confidential, proprietary > or otherwise private information. Any unauthorized use, reproduction, > dissemination, distribution or other disclosure of the contents of this > e-mail or its attachments is strictly prohibited. If you have received this > email in error, please notify the sender immediately and delete the > original. > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________