Hi Victor- While Steve gets your new photo up, I just glanced at the previous ones again since the link was below your latest message. The curious spots are the voids adjacent to the plating on the via walls--why didn't it plate into the voids? Is it possible the voids are created by your sectioning/polishing process? Wayne -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez Sent: Friday, August 28, 2015 12:02 PM To: [log in to unmask] Subject: [TN] Internal layer capture pad clearance Steve, Can you please post this photo for me. I would like to hear comments from our audience and their experience. What is the worst scenario? I am aware if IPC STD guidelines, 0.984 mil (0.025mm). Victor, From: Steve Gregory [mailto:[log in to unmask]] Sent: Friday, August 14, 2015 4:26 PM To: TechNet E-Mail Forum; Hernandez, Victor G Subject: Re: [TN] Pros & Cons om laminate VOIDS Hi Victor, Here you go: http://stevezeva.homestead.com/Laminate_voids.pdf Steve On Fri, Aug 14, 2015 at 12:23 PM, Victor Hernandez <[log in to unmask]<mailto:[log in to unmask]>> wrote: Fellow TechNetters: What are the Pros N Cons with LF laminate voids. Want to hear what the community thinks. I will upload photos to Steve Gregory shortly. Victor, Steve Gregory <[log in to unmask]<mailto:[log in to unmask]>> ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]> ______________________________________________________________________ [cid:[log in to unmask]] This email and any attachments are only for use by the intended recipient(s) and may contain legally privileged, confidential, proprietary or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly prohibited. If you have received this email in error, please notify the sender immediately and delete the original. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________