Hi Graham, I've used these for years: http://www.hunterproducts.com/Micro-Metallizer%20Catalog%20-%20Page%201.pdf They have everything you need, power supply, cleaning pens, nickel pens, and gold pens. Make sure you remove all the solder, careful scraping is best. Steve On Fri, Aug 21, 2015 at 5:19 AM, Graham Collins <[log in to unmask]> wrote: > Good day Technet > I've got some 20 boards that were badly taped and have solder on the gold > fingers. Aaarrrggg!!! > > So I know it is possible to get a kit with the chemicals and gear to allow > re-plating the fingers, we are looking at it but my questions are: > > 1) what is the best kit, does anyone have a recommendation (or warning)? > 2) does anyone offer this as a service? I've only got the 20 boards like > this, the cost per board will be fairly substantial and this has not > historically been a recurring issue. > > -- > regards, > > Graham Collins > Senior Process Engineer > Sunsel Systems > (902) 444-7867 > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > -- This email and any attachments are only for use by the intended recipient(s) and may contain legally privileged, confidential, proprietary or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly prohibited. If you have received this email in error, please notify the sender immediately and delete the original. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________