It looks like a solder resist repair and they used blue instead of green. It would be interesting to find out when the repair happened, at the board house or assembly house. It's difficult to tell because the silkscreen looks to be repaired as well. Ted T. Sent from my iPhone > On Jun 2, 2015, at 5:56 PM, Watson, Howard August <[log in to unmask]> wrote: > > Hi all, > > My PCB fab knowledge is limited, and a very unusual defect was discovered (too late) in assembly. I'm wondering if anyone has seen something like this before, or has an idea what this could be. The blue color seems noteworthy to me. This is for IPC class III, space. I will return this to the fabricator, but I wanted to get educated in case there is a debate regarding the cause. Thanks for your help! > > Steve put the pictures here: > > http://stevezeva.homestead.com/Howards_Blob.jpg > > http://stevezeva.homestead.com/Howards_Blob_close.jpg > Howard A. Watson > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________