It also takes into consideration the ideal paste printing conditions. Humidity and temperature both greatly affect the solder paste rheology, and thus directly affect printing performance, time on the stencil, etc. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey Sent: Monday, June 15, 2015 8:54 AM To: [log in to unmask] Subject: Re: [TN] Solder Paste ambient temperature and humidity The IPC recommendation for humidity is related to ESD control. The temperature recommendation is for operator comfort and solderability maintenance. J-SDT-001. 30%RH and 18-30 Celsius. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Avni Selim Özçukurlu Sent: Monday, June 15, 2015 4:54 AM To: [log in to unmask] Subject: [TN] Solder Paste ambient temperature and humidity Hello All, What should the average temperature and humidity level be in an electronic assembly and manufacturing facility? Especially, during solder paste print process to PCB, what is the ideal temperature and humidity? Is there any ipc standart? Note: We use Amtech NWS-4200. A.Selim ÖZÇUKURLU Aselsan MGEO - CCA Production and Test Engineer Tel: 90 312 847 53 00 / 4570 ###################################################################### Dikkat: Bu elektronik posta mesaji kisisel ve ozeldir. Eger size gonderilmediyse lutfen gondericiyi bilgilendirip mesaji siliniz. Firmamiza gelen ve giden mesajlar virus taramasindan gecirilmekte, guvenlik nedeni ile kontrol edilerek saklanmaktadir. Mesajdaki gorusler ve bakis acisi gondericiye ait olup Aselsan A.S. resmi gorusu olmak zorunda degildir. ###################################################################### Attention: This e-mail message is privileged and confidential. If you are not the intended recipient please delete the message and notify the sender. E-mails to and from the company are monitored for operational reasons and in accordance with lawful business practices. Any views or opinions presented are solely those of the author and do not necessarily represent the views of the company. ###################################################################### ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________