and yes, you need to use a dip formula. Regular stencil print solder paste will not dip well. Our supplier was very helpful with the selection. Roger Mack P.Eng. Manufacturing Specialist Parker Hannifin Canada Electronic Controls Division 1305 Clarence Avenue Winnipeg, MB R3T 1T4 Canada direct 204 453 3339 x7373 [log in to unmask] www.parker.com/ecd From: Roger Mack <[log in to unmask]> To: <[log in to unmask]> Date: 2015-06-29 02:07 PM Subject: Re: [TN] Solder Paste Dipping Ultra Fine Pitch QFPs for Reork? Sent by: TechNet <[log in to unmask]> I rework all BGA's using dip paste. Nice uniform coating covers the bottom half of the ball consistently. As BGA's got smaller stencil on part just never released cleanly. This also trades lots of stencils for a few thickness of dip trays. I make them so they fit on our stencil tray so the dip sequence runs on our VJ electronix (SRT) rework machine the same as picking any part out of a stencil. The dip sequence just adds an extra step to pick from one nest, then dip into the dip tray before placing on the board. We x-ray all reworked parts and this proved to be much more consistent. Have not yet tested dipping QFP's . The ones we rework have a center cooling plate to solder so we have had great results using the stick n peel stencil from BEST for that. Roger Mack P.Eng. Manufacturing Specialist Parker Hannifin Canada Electronic Controls Division 1305 Clarence Avenue Winnipeg, MB R3T 1T4 Canada direct 204 453 3339 x7373 [log in to unmask] www.parker.com/ecd From: Steve Gregory <[log in to unmask]> To: <[log in to unmask]> Date: 2015-06-29 01:44 PM Subject: Re: [TN] Solder Paste Dipping Ultra Fine Pitch QFPs for Reork? Sent by: TechNet <[log in to unmask]> Hi Bob, 10's of thousands? Wow. I have never used dipping pastes, but it would seem to me that you would definitely need some sort of automation to accomplish this, have you looked at automated lead tinning machines? Ace Production Technologies, RPS Automation, and Corfin Industries make lead tinning systems. I would also guess that the solder would tend to stay towards the bottom of the lead and not coat the entire lead with the dipping paste. Good luck! Steve Gregory On Mon, Jun 29, 2015 at 10:25 AM, Bob Wettermann <[log in to unmask]> wrote: > Hi All: > > We have a project where we need to rework 10's of thousands of LQFP > 100/0.5mm pitch devices. All options are being considered. > > Since the PoP dipping pastes have come in to their own has anyone tried > using these pastes to dip for fine pitch rework? > > Thanks! > > -- > Bob Wettermann > BEST Inc > > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > -- This email and any attachments are only for use by the intended recipient(s) and may contain legally privileged, confidential, proprietary or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly prohibited. If you have received this email in error, please notify the sender immediately and delete the original. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________