Hi Ioan, There can be many defects in wire bond, but it is typically limited to the critical defects for the process controls. We look for wire diameter, loop height, ball size, ball thickness, ball centering, wire length, pad cratering and wire pull data and ball shear data. Thank-you Mumtaz 858-795-0112 Peregrine Semiconductor -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea Sent: Wednesday, May 13, 2015 6:42 AM To: [log in to unmask] Subject: [TN] Wire bonding DPMO Dear Technos, Any of you using DPMO to track wire bonding process performance? I would like to know what are the defects you use to calculate your product DPMO, as wire bonding can produce tons of different defects, e.g. wire related (deformed, broken, poor loop, etc.), bond related (misformed, heel lift, offset, and so on). The more defects you consider, the lower the DPMO, as there are many more opportunities per unit. That would be a good indicator to show to customers, but in our case, we want to get a fair assessment of our processes, for our own process improvement use. So what are the defect opportunities I should count for one wire? Thanks, Ioan Tempea MDA Corporation ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ CONFIDENTIALITY NOTE: The information transmitted, including attachments, is intended only for the person(s) or entity to which it is addressed and may contain confidential and/or privileged material. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited. If you received this in error, please contact the sender and destroy any copies of this information. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________