Greetings fellow Technoids, An interesting debacle arose, and I'm unsure if there is a solution. Dpak components on side 1 solder fine, <25% voids, 100% edge wetting. On 2nd pass (top side, big heavy components) the Dpaks on side 1 outgas and exceed 25% (not a spec, just a target) but violate edge wetting (S/B 100%) as the outgas tends to blow out the edge somewhere. Any suggestion on how to eliminate this phenomena? Parts cannot be relocated due to aerospace re-qual cost. Thanks in advance! Ed Popielarski Engineering Manager [cid:[log in to unmask]] 970 NE 21st Ct. Oak Harbor, Wa. 98277 Ph: 360-675-1322 Fx: 206-624-0695 Cl: 949-581-6601 "It's one kind of victory to slay a beast, move a mountain, and cross a chasm, but it's another kind altogether to realize that the beast, the mountain, and the chasm were of your own design." https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________