Thanks Dave I suspected as much but wanted to check up on the current state of play. Best Regards Dr Lee Hitchens SCH Technologies is a Division of SCH Services Limited Mob: +44 (0) 7862 25 33 21 www.conformalcoating.co.uk <http://www.conformalcoating.co.uk/> TECHNICAL SUPPORT SERVICE SCH Services Ltd offers a Technical Support Helpline to help address all issues relating to reliability. This includes contamination testing, cleanliness and cleaning issues, plus any coating related questions. Please contact us via email or telephone: [log in to unmask] <mailto:[log in to unmask]> +44 (0)1226 249019 (office hours & answerphone) +44 (0)7862 253321(out-of-hours emergency) The opinions expressed in this e-mail are strictly those of the sender and not of SCH Services Limited. This communication may contain information which is confidential and may also be privileged. It is for the exclusive use of the intended recipient(s). Unauthorised use, copying or disclosure of any of it may be unlawful. If you are not the intended recipient(s) please note that any distribution, copying or use of this communication or the information in it is strictly prohibited. If you have received this communication in error please notify us by e-mail or by telephone (+44 (0)1226 249019) and then delete the e-mail and any copies of it. Virus Warning - Although steps have been taken to ensure that all email and attachments are virus-free, we cannot guarantee nor be held liable. Company Registration: 04043334 Registered office: SCH Services Limited Newburgh Building McLintock Way Barnsley South Yorkshire S70 6BF From: David Hillman <[log in to unmask]> Date: Thursday 7 May 2015 13:40 To: TechNet E-Mail Forum <[log in to unmask]>, Lee Hitchens <[log in to unmask]> Subject: Re: [TN] Conformal Coating Thickness Measurement on legs of components Hi Lee - as part of the IPC JSTD 001 "State of the Industry Assessment" of Conformal Coating Material & Application subcommittee activities, we looked at a number of conformal coating thickness measurement technologies/techniques since the test plan had 1,950 components to measure representing 26 material/application sets. We found several very adequate technologies for flat surfaces but as soon as you had a surface with any level of topography, the ability to measure coating thickness became very suspect. We settled on a very prescribed, rigid metallographic cross-sectional technique that is working very well other than it is slow and of course, destructive. I wish I had a better option for you but we didn't have any success in finding an adequate nondestructive method for nonflat surfaces. It is clearly a topic the industry needs and desires better method for measurement option. Dave Hillman Rockwell Collins [log in to unmask] On Thu, May 7, 2015 at 2:49 AM, Lee Hitchens <[log in to unmask]> wrote: > Hi all > > I am being asked regularly now on options for measuring coating thickness on > legs. I am trying to determine if there is actually a practical solution? > Cost is less important compared to being a workable relatively quick > process? > > One thing that could be an issue is many times its a silicone coating and > this tends to be less than clear optically. Some systems need clear coatings > to be successful. > > Has anyone had any success with this? > > Best Regards > > Dr Lee Hitchens > > SCH Technologies is a Division of SCH Services Limited > > Mob: +44 (0) 7862 25 33 21 <tel:%2B44%20%280%29%207862%2025%2033%2021> > > www.conformalcoating.co.uk <http://www.conformalcoating.co.uk> > <http://www.conformalcoating.co.uk/> > > > > > > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________