Thanks for all the feedback. It seems that there may be acceptable applications for transferring solder from the iron; specifically when you can inspect the result to be sure that you have gotten good wetting. Ben -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Ed Popielarski Sent: Wednesday, April 08, 2015 2:16 PM To: [log in to unmask] Subject: EXTERNAL: Re: [TN] Transfer Soldering http://store.curiousinventor.com/guides/Surface_Mount_Soldering/QFP/ Ed Popielarski Engineering Manager 970 NE 21st Ct. Oak Harbor, Wa. 98277 Ph: 360-675-1322 Fx: 206-624-0695 Cl: 949-581-6601 "It's one kind of victory to slay a beast, move a mountain, and cross a chasm, but it's another kind altogether to realize that the beast, the mountain, and the chasm were of your own design." https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Fenner Sent: Wednesday, April 08, 2015 10:44 AM To: [log in to unmask] Subject: Re: [TN] Transfer Soldering Possibly a problem with terms here. We usually think of transfer soldering as transfer printing of solder paste via pins, or other shaped tools from a controlled depth pool of solder to the work and then reflowing. I think what is meant in the question is melting a gob of solder onto 'iron bit (tip in US English) and then transferring to the work. This is usually not thought good technique as there is a tendency for the flux core to be burnt out on the tip before reaching the work. So extra flux could be applied to work, also improving thermal transfer, as remarked. It's possible for a good operator to obtain acceptable results in prototyping/low volume doing this. Higher volumes would merit a little more thought on designing a less craft like process. -- Best Wishes Mike -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of David Hillman Sent: Wednesday, April 08, 2015 2:45 PM To: [log in to unmask] Subject: Re: [TN] Transfer Soldering Ben - do you mean dippable solder paste? Dave Hillman Rockwell Collins [log in to unmask] On Wed, Apr 8, 2015 at 8:40 AM, Gumpert, Ben <[log in to unmask]> wrote: > Technetters, > > Anyone have comments on transfer soldering? > It's identified in an IPC video as one of the seven sins of soldering, > but seems to be focused on non-visible joints like through hole, as > opposed to SMT or wire soldering. > > There was a paper mentioned on Technet a while back which claimed > transfer soldering was just as good as 'normal' soldering, but there > was just a link > to the abstract. > > Ben > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or > [log in to unmask] > ______________________________________________________________________ > ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________