Are both of those tapes ESD safe? Ron -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls Sent: Thursday, April 02, 2015 10:38 AM To: [log in to unmask] Subject: Re: [TN] Masking tape recommendations for Acrylic conformal coating... I have always found that the brown polyimide plater's tape, found almost anywhere, is pretty good from a residue standpoint. The green polyester masking tape from Shercon is also pretty good. http://www.shercon.com/SherconTechPack/tape_pc21.html Doug Pauls Principal Materials and Process Engineer Rockwell Collins On Thu, Apr 2, 2015 at 10:08 AM, Steve Gregory <[log in to unmask]> wrote: > Morning All, > > I know this has been posted before, and for some reason I can't search > the archives. > > We're starting to do acrylic coating on some assemblies here, and I > was looking for some recommendations for masking tape that doesn't > leave residues. > > Can anybody give some recommendations? > > Steve > > -- > > > This email and any attachments are only for use by the intended > recipient(s) and may contain legally privileged, confidential, > proprietary or otherwise private information. Any unauthorized use, > reproduction, dissemination, distribution or other disclosure of the > contents of this e-mail or its attachments is strictly prohibited. If > you have received this email in error, please notify the sender > immediately and delete the original. > > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or > [log in to unmask] > ______________________________________________________________________ > ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________