Hi Jeff - here are a couple of other choices: 10Sn88Pb2Ag 1Sn97.5Pb1.5Ag 97Pb3Ag Nothing wrong with you 90Pb10Sn either. Make sure you select a flux core that has good thermal stability as your soldering temperatures are much hotter than what you deal with when using the Sn63Pb37 alloy. Also consider what the cleaning (or not cleaning) issues you may have to deal with. Dave Hillman Rockwell Collins [log in to unmask] On Wed, Apr 1, 2015 at 9:20 AM, McGlaughlin, Jeffrey A < [log in to unmask]> wrote: > I need to spec a high temperature wire solder for hand soldering. I need > to have a solidus of greater than 250 degrees C. Is 90Pb10Sn my best/only > choice or is there something else I should look at? > > Jeffrey McGlaughlin, C.I.D. > Engineering Designer > Avionics Systems & Tech Refersh > Office: 614.424.7582| Fax: 614.458.7582 > [log in to unmask]<mailto:[log in to unmask]> > > Battelle > 505 King Avenue > Columbus Ohio 43201-2693 > http://www.battelle.org<http://www.battelle.org/> > > Connect with Battelle > Facebook<http://www.facebook.com/battelle> | LinkedIn< > http://www.linkedin.com/company/battelle> > Twitter<http://www.twitter.com/Battelle> | YouTube< > http://www.youtube.com/user/battelleinnovations> > > This message is intended only for the use of the individual or entity to > which it is addressed, and may contain information that is privileged, > confidential and/or otherwise exempt from disclosure under applicable law. > If the reader of this message is not the intended recipient or the employee > or agent responsible for delivering the message to the intended recipient, > any disclosure, dissemination, distribution, copying or other use of this > communication or its substance is prohibited. If you have received this > communication in error, please return to the sender and delete from your > computer system. > > > > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________