It depends from alloy composition. BTW, the most common alloy LF have a melting point ranging from 217°C to 227°C. IPC/J-STD-006 shows all kinds of alloy's composition and related melting ponts Regards Gabriele -----Messaggio originale----- Da: TechNet [mailto:[log in to unmask]] Per conto di Victor Hernandez Inviato: mercoledì 4 febbraio 2015 18.06 A: [log in to unmask] Oggetto: [TN] LF Solder melting point Fellow TechNetters: At what temperature does LF solder began to melt? Victor, ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --- Questa e-mail è priva di virus e malware perché è attiva la protezione avast! Antivirus. http://www.avast.com ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________