I've seen this problem from time to time, and it can be a real headache. It seems like the fiducials are just the right size for this to be a problem with the HASL finish. Has anyone tried a different size fiducial, or different shape/pattern that might not have the same problem? (Although I'm sure anything different would cause problems with a lot of equipment.) Ben -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey Sent: Friday, September 05, 2014 11:34 AM To: [log in to unmask] Subject: EXTERNAL: Re: [TN] NOT Recognizing Panel Fiducials at paste printer. In my experience, the copper, without HASL is worse than the HASL, for those old printers and placers. We resorted to machine eraser. http://www.dickblick.com/products/sakura-cordless-electric-eraser/ We cleaned the board fiducials at receiving inspection. Gold will be more repeatable but I would think a switch from HASL to ENIG would be a major change. If it is a real simple design and HASL has good yields, I would expect ENIG to introduce more problems than it solves. It did in my case. We probably could have resolved the soldering problems by tweaking the reflow and wave settings. But, we went back to HASL. The buyer and the plant manager made the call. Immersion tin and immersion silver change color too. I bet your machines would have trouble with it. My experience with this problem dates back to the age of your old printers. Immersion Tin and Silver have been greatly improved since then. Wish I could be more help. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Jim West Sent: Friday, September 05, 2014 9:47 AM To: [log in to unmask] Subject: Re: [TN] NOT Recognizing Panel Fiducials at paste printer. Thanks for the replies. We build many thousands of this board so I was looking for a more permanent suggestion to give our board supplier. My thought was having the board supplier NOT apply solder (HASL) to the fiducials. Is this possible? Any other suggestion for a more permanent solution that our board house could implement without major changes (i.e. Immersion tin, or gold....). Major change would require an older board going through customer approval. Best Regards, Jim -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan TEMPEA Sent: Friday, September 05, 2014 7:52 AM To: [log in to unmask] Subject: Re: [TN] NOT Recognizing Panel Fiducials at paste printer. Jim, Removing the solder from the fiducials, using a solder wick, normally takes care of the issue. Regards, Ioan Tempea, P. Eng. Manufacturing Engineer Satellite Systems MDA 21025 TransCanada Highway Ste-Anne-de-Bellevue, Qc, Canada H9X 3R2 Tel: +1-514-457-2150-3556 www.mdacorporation.com This e-mail, and any attachments, are intended solely for the use of the intended recipient(s) and may contain legally privileged, proprietary and/or confidential information. Any use, disclosure, dissemination, distribution or copying of this e-mail and any attachments for any purposes that have not been specifically authorized by the sender is strictly prohibited. If you are not the intended recipient, please immediately notify the sender by reply e-mail and permanently delete all copies and attachments. -----Message d'origine----- De : TechNet [mailto:[log in to unmask]] De la part de Stephen Gregory Envoyé : Thursday, September 04, 2014 4:29 PM À : [log in to unmask] Objet : Re: [TN] NOT Recognizing Panel Fiducials at paste printer. Hi Jim, An old trick that I've used many times when the camera doesn't recognize a fiducial is to take a pencil eraser to it... Steve Sent from my BlackBerry 10 smartphone. Original Message From: Jim West Sent: Thursday, September 4, 2014 2:05 PM To: [log in to unmask] Reply To: TechNet E-Mail Forum Subject: [TN] NOT Recognizing Panel Fiducials at paste printer. Our paste printers are having difficulty recognizing the fiducials on an older board that has been running for years. The board house is applying HASL and because of that, as most are aware, the solder covering the fiducial pad will be inconsistent. I'm told that this has been an ongoing issue and the problem comes and goes. We have three printers that are older that do not allow us to adjust the lighting. I can't remember if we can have the board house apply HASL on just the component pads and not the fiducials? Any other suggestions? Thanks, Jim ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ -- This email and any attachments are only for use by the intended recipient(s) and may contain legally privileged, confidential, proprietary or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly prohibited. If you have received this email in error, please notify the sender immediately and delete the original. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________