Victor, You can also refer to IPC A-610E par. 7.3.5.9 pag. 7-53. Francesco Francesco Di Maio IPC A-600, IPC A-610, IPC 7711/21 Certified IPC Trainer "Gumpert, Ben" <[log in to unmask]> Sent by: TechNet <[log in to unmask]> 05/08/2014 15.56 Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to "Gumpert, Ben" <[log in to unmask]> To <[log in to unmask]> cc Subject Re: [TN] Post solder Component lead trimming Victor, J-STD-001 Rev E Para. 6.1.4 states that leads trimmed shall have the solder reflowed or inspected at 10X for damage. And if the trim cuts into the solder fillet, it must be reflowed. Ben -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez Sent: Tuesday, August 05, 2014 9:33 AM To: [log in to unmask] Subject: EXTERNAL: [TN] Post solder Component lead trimming Fellow TechNetters: Does IPC Standards address the lead trimming of components on post solder assemblies. I heard that on post solder lead trimming that a second pass solder operation is required to ensure solder joint integrity from the lead trimming process. Any comments and/or direction for literature review. Victor, ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________